PPGI vs PPGL: What Is the Difference?
PPGI is pre-painted steel on a hot-dip zinc (Z) substrate and PPGL is pre-painted steel on a 55% aluminium-zinc (AZ) substrate; the paint can be the same, so the difference is the metallic coating underneath.
Produced in our group's own mills, inspected and shipped by Kexinda. Mill test certificate (EN 10204 3.1), issued by our group mill, available on request.
PPGI vs PPGL side by side
| PPGI (pre-painted galvanized) | PPGL (pre-painted aluminium-zinc) | |
|---|---|---|
| Metallic coating under the paint | Hot-dip zinc (code Z) | Hot-dip aluminium-zinc, about 55% Al, 43.4% Zn, 1.6% Si (code AZ) |
| How the coating protects | Zinc corrodes first and protects the steel (sacrificial protection) | Barrier plus electrochemical protection; higher corrosion resistance than zinc in most environments, better heat resistance and heat reflection |
| Common substrate coating for roof and wall sheet | Z180–Z275 (g/m², both sides) | AZ100–AZ150 (g/m², both sides) |
| Grade written as (GB/T 12754) | T + substrate grade, e.g. TDX51D+Z | T + substrate grade, e.g. TS300GD+AZ |
| Substrate standard | GB/T 2518 (Z); ASTM A653/A653M; EN 10346 (+Z) | GB/T 2518 (AZ); ASTM A792/A792M; EN 10346 (+AZ) |
| Pre-painted standard | GB/T 12754-2019; ASTM A755/A755M; EN 10169 | GB/T 12754-2019; ASTM A755/A755M; EN 10169 |
| Paint (both) | Top-side coating at least 20 micron in total; back 5 micron (one layer) or 12 micron (two layers), per GB/T 12754 | Same paint rules |
| HS code (6 digits) | 7210.70 (600 mm or wider) | 7210.70 (600 mm or wider) |
How to choose
- Start from the site: GB/T 12754 Annex B lists the corrosivity of the use environment, the life to first major maintenance and the forming method as the main factors for choosing substrate, coating mass and paint.
- Coating mass matters as much as the type: state the mass on the order (for example Z275 or AZ150), not only "PPGI" or "PPGL". See zinc coating Z80 to Z275.
- Paint film: GB/T 12754 requires at least 20 micron in total on the top-side coating; thicker paint generally lasts longer.
What to send for a quotation
- PPGI or PPGL, substrate grade and coating mass (e.g. DX51D+Z275 or S350GD+AZ150)
- Thickness, width, coil inner diameter and coil weight
- Paint system, colour (RAL number) and film thickness (top-side and back)
- Quantity and destination port
Product page: PPGI / PPGL pre-painted coil · GI coil · GL coil
Frequently asked questions
Which is better, PPGI or PPGL?
Neither in every case. GB/T 2518 describes aluminium-zinc (the PPGL substrate) as more corrosion resistant than zinc in most environments, while zinc (PPGI) gives sacrificial protection. Choose by the corrosivity of the site and the required life to first maintenance, as GB/T 12754 Annex B advises.
How can I tell PPGI from PPGL on a mill certificate?
Look at the grade: GB/T 12754 writes T plus the substrate grade, so +Z means a zinc (PPGI) substrate and +AZ an aluminium-zinc (PPGL) substrate, for example TDX51D+Z or TS300GD+AZ.
Do PPGI and PPGL use the same paints?
Yes. Both are offered with polyester (PE), silicone-modified polyester (SMP), high-durability polyester (HDP) and PVDF paint; GB/T 12754 sets the same minimum film thickness for both.
Is the HS code different?
No. Pre-painted flat-rolled steel 600 mm or wider is 7210.70 whether the substrate is zinc or aluminium-zinc. See our HS codes guide.
Sources
- GB/T 2518-2019 English edition excerpt (PDF), chinesestandard.net – coating codes Z and AZ; Annex B.3: zinc gives sacrificial protection; aluminium-zinc has higher corrosion resistance in most environments, better heat resistance and heat reflection
- GB/T 12754-2019 English edition excerpt (PDF), chinesestandard.net – grade = T + substrate grade (e.g. TDX51D+Z, TS300GD+AZ); top-side coating at least 20 micron; back 5 / 12 micron; selection by environment (Annex B)
- GB/T 12755-2008 listing, chinesestandard.net – minimum substrate coating for profiled sheet (basis of the Z180–Z275 / AZ100–AZ150 range)
- GalvInfo Center, GalvInfoNote 1.1 (coating mass designations) – coating mass designations, total both sides
- ASTM A755/A755M scope page – ASTM A755/A755M scope
- EN 10169:2022 listing, iTeh – EN 10169 scope
- ASTM A792/A792M-21 scope page – ASTM A792 aluminium-zinc coated sheet
- WCO, HS Nomenclature 2022, Chapter 72 (Iron and steel) – Note 1(k) on flat-rolled products; subheadings 7210.41, 7210.49, 7210.61, 7210.70, 7212.40, 7216.61, 7216.91
Sources checked on 5 November 2026. Values marked calculated are worked out from the formula shown, not copied from a table. Typical industry ranges; we confirm the exact values for your order.
Get a Quote for PPGI / PPGL Pre-painted Coil
Send your drawing or size list; we reply with a price.
Working hours: Mon–Sat 8:30–17:30 Beijing time (UTC+8).
Or email sales01@kexinda-industry.com
What a quotation from us includes: see a blank quotation sample.