C Purlin Sizes Explained

A C purlin size is written as web height x flange x lip x thickness in mm; the designation (C80 to C250) gives the web height, and the other three numbers complete the section.

C purlin dimensions H, B, C, tB flangeHC lipt = thicknessIllustrative - not to scale
H = web height, B = flange width, C = lip, t = thickness. Illustrative.

How to read a C purlin size

C section list

The web height is given by the designation. We produce every section in this table with the flange, lip and thickness shown; other sizes: send your drawing, we confirm sizes in the quotation.

SectionWeb height H (mm)Flange B (mm)Lip C (mm)Thickness t (mm)
C808040152.0–3.0
C10010050202.0–3.0
C12012050202.0–3.0
C14014050202.0–3.0
C15015060202.0–3.0
C16016060202.0–3.0
C18018060202.0–3.0
C20020060202.0–3.0
C25025070202.0–3.0

Weight per metre

Sectiont = 2.0 mm (kg/m)t = 2.5 mm (kg/m)t = 3.0 mm (kg/m)
C802.863.534.19
C1003.644.515.37
C1203.964.915.84
C1404.275.306.31
C1504.745.897.02
C1604.906.087.25
C1805.216.487.72
C2005.536.878.20
C2506.638.249.84

Calculated from the nominal dimensions above (centre-line length of the section x thickness x 7.85 kg/dm³), rounded; zinc coating not included. Real sections weigh slightly more or less; your invoice uses the weighed or calculated weight agreed in the quotation.

Standards and design codes

Steel grade and zinc coating

Grade (EN 10346)Min. yield (MPa)Closest ASTM A653 grade, by yield only
S350GD+Z350SS Grade 50 (about 345 MPa)
S550GD+Z550Grade 80 (about 552 MPa)
Zinc coating systemDesignations
EN 10346Z100, Z140, Z200, Z225, Z275, Z350, Z450, Z600 (g/m², both sides)
ASTM A653M / A653Z90, Z120, Z180, Z275, Z350 / G30, G40, G60, G90, G115; G90 = Z275

Equivalents are the nearest published standard or grade, matched by scope or by yield strength only. They are a nearest equivalent, not a certification. Our product pages reference these standards; mill certificates and test reports are available on request where applicable.

What to send for a quotation

See also: C purlin product page · Z vs C purlin

Frequently asked questions

What does C160 mean?

A C section with a 160 mm deep web. The full size also needs the flange width, lip length and thickness, e.g. H x B x C x t.

Are deeper C sections available?

Our table runs from C80 to C250. For deeper sections, send your drawing; we confirm sizes in the quotation.

Which steel grade should I specify?

Your designer specifies it. For reference, EN 10346 S350GD+Z (350 MPa minimum yield) sits closest to ASTM A653 SS Grade 50, and S550GD+Z to Grade 80, by yield only.

Sources

  1. SAMR National Public Service Platform for Standards Information, GB/T 6728-2025 record – GB/T 6728-2025 Cold-formed steel sections for general structure: status in force, issued 2025-08-29, in force from 2026-03-01
  2. SAMR National Public Service Platform for Standards Information, GB/T 6723-2017 record – GB/T 6723-2017 General cold-formed open steel sections: status withdrawn

Standard status checked on 5 November 2026 on std.samr.gov.cn: GB/T 6723-2017 withdrawn, GB/T 6728-2025 in force. Typical industry ranges; we confirm the exact values for your order.

Request a Quote

Send your drawing or size list; we reply with a price.

Working hours: Mon–Sat 8:30–17:30 Beijing time (UTC+8).

Email us

Or email sales01@kexinda-industry.com

What a quotation from us includes: see a blank quotation sample.

Fill in what you know; the form opens WhatsApp or your email with the message ready to send.

You can attach your drawing or BOQ in WhatsApp or email after the message opens.